Welding:INCOLOY alloy 800 can be welded by common welding techniques, using a matching filler metal.
Forming:This alloy exhibits good ductility and hence can be formed using conventional methods.
Hot working:INCOLOY alloy 800 can be hot worked at temperature ranges of 871-1232°C (1600-2250°F).
Cold Working:Cold working may be done on the alloy using standard tooling.
Annealing:INCOLOY alloy 800 may be annealed after cold working. Annealing should be done at 982°C (1800°F) for 15 min and then the alloy should be air cooled.